TISCO INDUSTRIAL CO.,LIMITED can produce boiler and pressure vessel according to: GB713, GB3531, GN18189, GB24510, EN10028, ASME SA387, SA515, SA516, SA537 etc., can also produce HIC and SSCC resistant plate, such as Q345(R-HIC), A516GR60N(HIC), 12Cr2Mo1R(H), P265GH, 13MnNiMo54 etc..
Typical Steel Grades/Specifications
Grade |
Specification |
Size Range (mm) |
Delivery Condition |
Q245R |
GB 713 |
6-200 |
AR,CR,N |
Q345R |
GB 713 |
6-200 |
AR,CR,N |
Q370R |
GB 713 |
10-60 |
N |
15CrMoR |
GB 713 |
6-150 |
N+T |
14Cr1MoR |
GB 713 |
6-150 |
N+T |
12Cr2Mo1R |
GB 713 |
6-200 |
N+T |
12Cr2MoVR |
GB 713 |
6-150 |
N+T |
16MnDR |
GB 3531 |
8-120 |
N+T |
09MnNiDR |
GB 3531 |
6-120 |
N+T |
12MnNiVR |
GB 19189 |
10-45 |
Q+T |
06Ni9DR |
GB 150 |
5-50 |
NNT,QT,QLT |
SA387Gr11 |
ASME SA387 |
6-150 |
N+T |
SA387Gr12 |
ASME SA387 |
6-150 |
N+T |
SA387Gr22CL1 |
ASME SA387 |
6-150 |
N+T |
SA387Gr22CL2 |
ASME SA387 |
6-200 |
N+T |
SA204GrA |
ASME SA204 |
6-150 |
AR,N |
SA204GrB |
ASME SA204 |
6-150 |
AR,N |
SA204GrC |
ASME SA204 |
6-100 |
AR,N |
SA515Gr60 |
ASME SA515 |
6-200 |
AR,CR,N |
SA515Gr65 |
ASME SA515 |
6-200 |
AR,CR,N |
SA515Gr70 |
ASME SA515 |
6-200 |
AR,CR,N |
SA516Gr55 |
ASME SA516 |
6-305 |
AR,CR,N |
SA516Gr60 |
ASME SA516 |
6-205 |
AR,CR,N |
SA516Gr65 |
ASME SA516 |
6-205 |
AR,CR,N |
SA517Gr70 |
ASME SA516 |
6-406 |
AR,CR,N |
SA537CL1 |
ASME SA537 |
6-100 |
N |
SA537CL2 |
ASME SA537 |
6-100 |
QT |
P355GH |
EN 10028-2 |
6-150 |
N |
P265GH |
EN 10028-2 |
6-150 |
N |
P355NH |
EN 10028-3 |
6-150 |
N |
P355NL1 |
EN 10028-3 |
6-150 |
N |
16Mo3 |
EN 10028-3 |
6-150 |
N |
13CrMo4-5 |
EN 10028-2 |
6-290 |
N+T,Q+T |
Q245(R-HIC) |
GB 713 |
6-100 |
N |
Q345(R-HIC) |
GB 713 |
6-180 |
N |
15CrMoR(H) |
GB 713 |
6-150 |
N+T |
14Cr1MoR(H) |
GB 713 |
6-150 |
N+T |
12Cr2Mo1R(H) |
GB 713 |
6-200 |
N+T |
A516GR60N(HIC) |
ASME SA516 |
6-120 |
N |
A516GR70N(HIC) |
ASME SA516 |
6-180 |
N |
34CrMo4 Gas Cylinder Steel |
EN 10083 |
6-10 |
AR |
(1) 12 Cr2Mo1R(H) Chemical Composition
Grade |
Chemical Composition(wt%) |
||||||||||||
C |
Si |
Mi |
P |
S |
Cr |
Ni |
Mo |
Cu |
As |
Sb |
Sn |
[H] |
|
12Cr2Mo1R(H) |
≤0.15 |
≤0.15 |
0.30-0.60 |
≤0.010 |
≤0.010 |
2.0-2.5 |
≤0.20 |
0.90-1.10 |
≤0.20 |
≤0.016 |
≤0.003 |
≤0.015 |
≤2ppm |
Mechanical Properties
Size(mm) |
Rp0.2,Mpa(℃) |
Rm,Mpa(℃) |
A%(℃) |
Z(%) |
AKV(-30℃),J |
Bend Test |
125 |
≥310 |
515-690 |
≥18 |
≥45 |
≥54 |
180° d=3a, ok |
HIC test standard: NACE TM0284 or GB/T8650. The HIC test can be carried out in Wuxi Sunny Xinrui Steel Group., Ltd inspection center, or third party inspection lab. The test report can be provided.
SSCC test standard: NACE TM0177 or GB/T4157. The SSCC test can be carried out in Wuxi Sunny Xinrui Steel Group., Ltd inspection center, or third party inspection lab. The test report can be provided.